Product Profile of Low Antimonial Lead Alloy
Low Antimonial Lead Alloy has eutectic melting point at 253 ° C with 11.1 % antimony by weight. The Alloy has good castability and ensures increase of hardness and tensile strength. The Low Antimonial Lead Alloy has tin content from 0.15% to 0.5%.
Key Features of Low Antimonial Lead Alloy
- Eutectic melting point at 253 ° C with 11.1 % antimony by weight.
- Good castability and ensures increase of hardness and tensile strength.
- Tin content from 0.15% to 0.5%.