Industrial Grade Sulphomor Sulphur Mortar is resistant to non-oxidizing acids, dilute oxidizing acids and neutral salts. The Mortar has density of cured mortar of 2.10 grm/ cc to 2.20 grm/ cc, bond strength of 10 kg/ cm2, compressive strength of 280 kg/ cm2, flexural strength of 70 kg/ cm2. The Mortar has resistant to temperature of 90 ° C. The Mortar should be heated at low temperature in a suitable kettle by stirring with metal rod or ladle and the surface shall be laid first with membrane. The Industrial Grade Sulphomor Sulphur Mortar is poured between the wall surface and the tile or bricks and please ensures that no water shall be spilled over the bricks lining works before it completely cured.