Key Features of Acrylonitrile Butadiene Styrene
- Extrusion temperature: from 210 to 240 C
- L/D ratio of 25-30
- Drying before processing is highly recommended
- Moisture content should be a maximum of 0.2%.
- The maximum permissible drying temperatures lie in the range of about 80 to 110 degree C.
- PA6 is thermally stable up to 310 C, but above decomposition accelerates, the initial products formed